CHEMICAL ANALYSIS
PHYSICAL-MECHANICAL CHARACTERISTICS
Compressive strength ( Kg/cm²) | 1689 |
Compressive strength after ice ( kg/cm² ) | Sem alteração (48 C.) |
Resistance to bending ( kg/cm²) | 16.2 |
Apparent volumetric mass (kg/cm²) | 2621 |
Water absorption PTN | 0.5% |
Open porosity | 1.4% |
FINISHING
- Polished
- Honed
- Sandblasted
- Bush-hammered
- Split
- Brushed
- Flamed